Yb: YAG レーザー結晶
仕様
◀︎表は横にスクロールして見ることができます▶︎
製品検索


| Materials | Yb:YAG | 
| Yb Concentration Tolerance (atm%) | 0.5, 1, 2, 3, 5, 7.5 , 10, 15, 20, 25% | 
| Orientation | [001] or [110] or [111] <±0.5° | 
| Parallelism | 10〞 | 
| Perpendicularity | 5ˊ | 
| Surface Quality | 10-5(MIL-O-13830A) | 
| Wavefront Distortion | λ/4@632nm | 
| Surface Flatness | λ/8@632nm | 
| Clear Aperture | >95% | 
| Chamfer | <0.1×45° | 
| Thickness/Diameter Tolerance | ±0.05 mm | 
| Maximum Dimensions | dia 50×100 mm | 
| Coatings | AR/AR@940+1030;HR@940+AR1030 | 
| Crystal Structure | cubic – la3d | 
| Lattice Constants | 12.01 Å | 
| Density | 4.56±0.04 g/cm3 | 
| Melting Point | 1970 °C | 
| Thermal Conductivity /(W·m-1·K-1@25°C) | λ/4@632nm | 
| Specific Heat/ (J·g-1·K-1) | 0.59 | 
| Thermal Optical Coefficient(dn/dT) | 7.3×10-6/℃ | 
| Thermal Expansion /(10-6·K-1@25°C ) | 8.2 [100] 7.7 [110] 7.8 [111] | 
| Hardness (Mohs) | 8.5 | 
| Young`s Modulus /GPa | 317 | 
| Shear Modulus /Gpa | 54.66 | 
| Extinction Ratio | 25 dB | 
| Tensile Strength/Gpa | 0.13-0.26 | 
| Solubility | Water: Insoluble; Common Acides: Slightly | 
| Poisson Ratio | 0.25 | 
| Laser Transition | 2F5/2→2F7/2 | 
| Laser Wavelength | 1030 nm | 
| Photon Energy | 1.93×10-19J(@1030 nm) | 
| Pump Absorption Band Width | 8 nm | 
| Loss Coefficient | 0.003 cm-1 | 
| Diode Pump Band | 940 nm or 970 nm | 
| Emission Cross Section | 2.0×10-20 cm2 | 
| Fluorescence Lifetime | 1.2 ms | 
| Emission Linewidth | 9 nm | 
| Refractive Index @1.030 μm | 1.82 | 
| Thermal Optical Coefficient | 9× 10-6/℃ | 
◀︎表は横にスクロールして見ることができます▶︎
メーカー紹介Crylink
Crylink
◆ 広いチューナブル波長領域 (650-1100nm)
◆ 広い吸収波長領域
◆ 優れた出力効率
◆ 短い励起寿命
◆ 高いダメージ閾値
Crylink
◆ 2.94μm 発振波長 (高い水への吸収性)
◆ 低い潮解性
◆ 広い透明度
◆ 高いダメージ閾値
◆ 安定した化学的および物理的特性
Crylink
◆ 946nm, 1064nm, 1120nm, 1320nm, 1440nm 発振
◆ 広い吸収帯域幅
◆ 低い発振閾値
◆ 優れた光学的、機械的、物理的特性
◆ 高いゲイン係数