| Concentration Tolerance (atm%) | 0.5%, 1.1%, 2.0%, 3.0% |
| Orientation | A-cut or C-cut |
| Parallelism | 20〞 |
| Perpendicularity | 5〞 |
| Surface Quality | 10/5 Scratch/Dig per MIL-O-13830 B |
| Wavefront Distortion | <λ/8 @633nm |
| Surface Flatness | λ/10@ 633 nm |
| Clear Aperture | >90% |
| Chamfer | ≤0.2mm@450 |
| Dimension Tolerance | (W±0.1mm)x(H±0.1mm)x(L+0.2/-0.1mm) (L<2.5mm) |
| (W±0.1mm)x(H±0.1mm)x(L+0.5/-0.1mm) (L≥2.5mm) | |
| Angle Tolerance | ≤0.5° |
| Damage Threshold[GW/cm2 ] | >1 for 1064nm, TEM00, 10ns, 10Hz (AR-coated) |
| Coatings | HR@1064nm+532nm+HT@808nm/AR@1064nm+532nm |
| Crystal Structure | Zircon Tetragonal, space group D4h-I4/amd |
| Lattice Constants | a=b=7.12, c=6.29 |
| Density | 4.22g/cm3 |
| Melting Point | 1825 |
| Thermal Conductivity /(W·m-1·K-1@25°C) | 5.2 |
| Thermal Optical Coefficient(dn/dT) | dno/dT=8.5×10-6/K; dne/dT=2.9×10-6/K |
| Thermal Expansion /(10-6·K-1@25°C ) | a = 4.43, c= 11.4 |
| Hardness (Mohs) | 4~5 |
| Laser Wavelength | 1064nm, 1342nm |
| Polarized Laser Emission | π polarization; parallel to optic axis (c-axis) |
| Pump Wavelength | 808nm |
| Intrinsic Loss | 0.02cm-1 @1064nm |
| Diode Pumped Optical to Optical Efficiency | >60% |
| Emission Cross Section | 25×10-19cm2@1064nm |
| Fluorescence Lifetime | 90 μs (about 50 μs for 2 atm% Nd doped) @ 808 nm |
| Gain Bandwidth | 0.96nm @1064nm |
| Refractive Index | 1.9573(no); 2.1652(ne) @1064nm |
| 1.9721(no); 2.1858(ne) @808nm | |
| 2.0210(no); 2.2560(ne) @532nm | |
| Absorption Coefficient | 31.4 cm-1 @ 808 nm |
| Absorption Length | 0.32 mm @ 808 nm |
| Gain Bandwidth | 0.96 nm (257 GHz) @ 1064 nm |
◀︎表は横にスクロールして見ることができます▶︎
メーカー紹介Crylink
Crylink
◆ 広いチューナブル波長領域 (650-1100nm)
◆ 広い吸収波長領域
◆ 優れた出力効率
◆ 短い励起寿命
◆ 高いダメージ閾値
Crylink
◆ 2.94μm 発振波長 (高い水への吸収性)
◆ 低い潮解性
◆ 広い透明度
◆ 高いダメージ閾値
◆ 安定した化学的および物理的特性
Crylink
◆ 1030nm発振
◆ 直線偏光発振
◆ シングルモード発振
◆ 広い吸収帯域と広い発光範囲
◆ 高い光学品質